Technical Specification Table
| Property |
Method |
SI Unit |
SI Value |
| Density |
ASTM D-792 |
g/cm3 |
0.953 |
| Yield Point |
ASTM D-638 |
MPa |
20 |
| Elongation at Yield |
ASTM D-638 |
% |
15 |
| Tensile Break |
ASTM D-638 |
MPa |
45 |
| Elongation at Break |
ASTM D-638 |
% |
290 |
| Tensile Modulus |
ASTM D-638 |
MPa |
913 |
| Flexural Modulus |
ASTM D-790 |
MPa |
723 |
| Izod Impact (Charpy Notched Impact) |
ASTM D-4020 |
kJ/m2 |
113 |
| Tensile Impact |
DIN 53448 |
kJ/m2 |
3096 |
| Sand Wheel Wear |
ASTM G-65 |
T-1000=100 |
113 |
| Hardness |
ASTM D-2240 |
Shore D |
69 |
| Static Friction |
ASTM D-1894 |
Unitless |
0.18 |
| Dynamic Friction |
ASTM D-1894 |
Unitless |
0.15 |
| Coefficient of Thermal Exp |
ASTM D-696 |
°C-1 |
0.00018 |
| Melt Point |
ASTM D-3417 |
°C |
137-143 |
| Compressive Modulus |
ASTM D-695 |
MPa |
na |
| Compressive Deformation |
ASTM D-621 |
% at 454.5kg |
na |
| Volume Resistivity |
ASTM D-257 |
Ohm-cm |
>1015 |
| Surface Resistivity |
ASTM D-257 |
Ohm |
>1015 |
| Water Absorption |
ASTM D-5706 |
% |
nil |
| |